MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Scotchcal™ 50-64 Graphic Film
Categories: Polymer; Film

Material Notes: Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a white liner on all other film colors. Use this versatile film in both indoor and outdoor applications for thermal mass transfer and electronic cutting. It is removable with heat for up to three years and permanent for up to five years. This 3-mil film may be printed with thermal mass transfer and electronically cut.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 76.2 microns3.00 milwithout adhesive
 102 - 114 microns4.00 - 4.50 milwith adhesive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 18.4 MPa>= 2670 psi
Peel Strength 0.526 kN/m3.00 pliAdhesion to Glass
 0.701 kN/m4.00 pliAdhesion to Acrylic
 0.701 kN/m4.00 pliAdhesion to Fruehauf pre-painted panel
 0.701 kN/m4.00 pliAdhesion to Polycarbonate
 0.877 kN/m5.00 pliAdhesion to Alodine, aluminum
 
Processing PropertiesMetricEnglishComments
Processing Temperature 4.00 - 38.0 °C39.2 - 100 °FApplication Temperature
 
Descriptive Properties
AppearancePink

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35014 / 169761

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.