MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Pyrotek Pyrocast L-30 Moldable Refractory
Categories: Ceramic

Material Notes: Pyrocast L-30 is a refractory moldable designed for use in contact with molten aluminum. Pyrocast L-30 has excellent workability for use as an insulating lining or patching material and is recommended for thicknesses up to 50 mm (2 in). If applied above 20°C, Pyrocast L-30 adheres well to metal and refractory surfaces.

Applications

  • Coatings
  • Linings
  • Refractory patching
  • Sealing compound
  • Collector bar seals

Advantages

  • Non-wetting
  • Good adhesion qualities
  • Low shrinkage
  • Low thermal conductivity

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.640 g/cc0.0231 lb/in³
Solids Content 55 %55 %
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0800 W/m-K
@Temperature 204 °C
0.555 BTU-in/hr-ft²-°F
@Temperature 399 °F
 0.160 W/m-K
@Temperature 538 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 0.220 W/m-K
@Temperature 871 °C
1.53 BTU-in/hr-ft²-°F
@Temperature 1600 °F
Maximum Service Temperature, Air 1093 °C1999 °F
Shrinkage  2.0 %
@Temperature 1093 °C,
Time 86400 sec
2.0 %
@Temperature 1999 °F,
Time 24.0 hour
linear
 6.0 %
@Temperature 1260 °C,
Time 86400 sec
6.0 %
@Temperature 2300 °F,
Time 24.0 hour
 
Descriptive Properties
Hot Gas Erosion ResistanceMin 61 m/sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications
Pyrotek Pyrocast AR70 Low-Density Refractory Castable
Pyrotek Pyrocast AR-S Castable Refractory
Pyrotek Pyrocast AR PLUS Castable Refractory
Pyrotek Pyrocast HD Castable Refractory

CPYRO037 / 1799

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.