MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik VESTAMID® LX9012 Bio30 Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID LX9012 Bio30 is a semi-crystalline, heat- and UV-stabilized compound based on PA12. The material was developed for the use in injection molding and is especially suitable for sport and lifestyle applications. The semi-crystalline compound only absorbs small amounts of water. Therefore, components made of this material have excellent dimensional accuracy under changing ambient humidity and are durably scratch-resistant. VESTAMID LX9012 Bio30 is delivered as cylindrical pellets in ready-to-process condition in moisture-tight bags. Preliminary data sheet. The use of colorants can change the property values.
Dry properties listed below
Industrial Sector: Automotive Sustainable, Sports and Lifestyle
Sustainability: Sustainable electricity
Processing: Injection molding
Delivery form: Pellets, Granules
Optics: Translucent
Resistance to: Heat (thermal stability), UV / light / weathering
Electrical: Insulating
Additives: Unfilled
Applications: General purpose
Processing: Thermoforming
Special Characteristics: Semi-crystalline, U.V. stabilized
Color: Natural color
Additives: Heat stabilizer
Delivery form: Cylindrical pellets
Chemical Resistance: General chemical resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Water Absorption 0.290 %
@Time 86400 sec
0.290 %
@Time 24.0 hour
ISO 62, ASTM D 570
Linear Mold Shrinkage, Flow 0.0110 cm/cm0.0110 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0110 cm/cm0.0110 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 73.073.0ISO 7619-1
Tensile Strength at Break 44.0 MPa6380 psiISO 527
Tensile Strength 45.0 MPa6530 psiISO 527
Tensile Stress 31.0 MPa
@Strain 50.0 %
4500 psi
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 38.0 MPa5510 psiISO 527
Elongation at Break 233 %233 %Nominal; ISO 527
 239 %239 %ISO 527
Elongation at Yield 5.00 %5.00 %ISO 527
Tensile Modulus 1.17 GPa170 ksiISO 527
Flexural Strength 33.0 MPa4790 psiat conv. Deflection; ISO 178
 44.0 MPa6380 psiISO 178
Flexural Modulus 0.951 GPa138 ksiISO 178
Flexural Strain at Break 8.00 %8.00 %at flexural strength; ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 176 °C349 °FISO 11357-1/-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °F
Mold Temperature 60.0 °C140 °F
 
Descriptive Properties
Blue water consumption572.8 kgISO 14040, 14044
ColorNatural Color
Global Warming Potential1.7 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 6.7 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 7.5 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)7.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7920 / 325052

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.