MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; A (A) Temper; All Sizes (UNS N03360)  (discontinued **)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Nickel Alloy

Material Notes: Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.28 g/cc0.299 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 760 MPa>= 110000 psi
Tensile Strength, Yield >= 345 MPa>= 50000 psi
Elongation at Break >= 45 %>= 45 %
Modulus of Elasticity 207 GPa30000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000430 ohm-cm0.0000430 ohm-cm4% IACS Conductivity
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 - 200 °C
7.78 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 48.0 W/m-K333 BTU-in/hr-ft²-°F
Melting Point 1196 - 1330 °C2185 - 2430 °F
Solidus 1196 °C2185 °F
Liquidus 1330 °C2430 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 1.85 - 2.05 %1.85 - 2.05 %
Nickel, Ni 97.5 %97.5 %as balance
Titanium, Ti 0.40 - 0.60 %0.40 - 0.60 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H1050 (H1050) Temper; All Sizes (UNS N03360)
Copper, Cu; Cold Drawn
Copper, Cu; Annealed
Copper, Cu; Cold-Worked
Dezincification Brass, DZR, UNS C35330

NBB770 / 15306

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.