MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wynca WynPh ® FR720 Halophosphate-free Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Advantages:
  • Specifically suitable for glass fiber reinforced and non-enhanced polyester systems.
  • Flexible combination with a variety of co-active agents, can meet the requirements of UL 94 V-0 flame retardant.
  • There are excellent physical properties and electrical properties in the application of flame retardant polyester system.
  • Halogen-free flame retardant, safe and environmental protection, to meet the requirements of RoHS and REACH regulations.
Application and Suggestion:Halogen-free flame retardant FR720 can be combined with a variety of synergistic agents based on customer characteristics, to realize the glass fiber enhanced or non-enhanced polyester system flame retardant UL94 V-0 (1.6,0.8,0.4mm, etc.) standard. According to the polymer specifications, processing conditions, glass fiber content and flame retardant level requirements, the dosage of flame retardant should be adjusted appropriately, and it is recommended to add 15-20 parts.

Information provided by Wynca Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.30 %<= 0.30 %
Grain Size 25 µm25 µmD50
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature >= 350 °C>= 662 °F
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 23 - 24 %23 - 24 %
 
Descriptive Properties
AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWYNCA084 / 320642

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.