MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

AISI 1139 Steel Composition Spec (UNS G11390)
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Key Words: UNS G11390
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.35 - 0.43 %0.35 - 0.43 %
Iron, Fe 97.68 - 98.17 %97.68 - 98.17 %As Balance
Manganese, Mn 1.35 - 1.65 %1.35 - 1.65 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S 0.13 - 0.20 %0.13 - 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
409 Stainless Steel
AISI 1141 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1144 Steel, annealed at 790°C (1450°F), furnace cooled 11°C (20°F) per hour to 620°C, air cooled, 25 mm (1 in.) round
AISI 1146 Steel Composition Spec (UNS G11460)
AISI 1340H Steel, annealed at 800°C, furnace cooled 11°C/hour to 600°C, air cooled, 25 mm (1 in.) round

M1139 / 100206

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.