MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Network Polymers 351 Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes: Description: Ignition Retardant

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccASTM D792
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Procedure A Condition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4200 psiASTM D638
Elongation at Break 30 %ASTM D638
Flexural Strength 5700 psiASTM D790
Flexural Modulus 275000 psiASTM D790
Izod Impact, Notched 1.70 ft-lb/inInjection Molding; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 187 °FASTM D648
Vicat Softening Point 100 °CASTM D1525
Flammability, UL94 V-0
@Thickness 1.59 mm
 
Descriptive Properties
Color Stabilitymin 10Change in E at 300 hours; ASTM D4459

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei Xyron™ X404H PPE/PS, High Stiffness, Ultra Low Warp Chassis
Chi Mei Polyrex® PG-22 Polystyrene
Network Polymers NPS 80-0201 Crystal Polystyrene
Versalis Extir® LN 2000 Expandable Polystyrene
American Polymers API 550 Polystyrene

PDIAM058 / 29896

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.