MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NaturePlast PLE 005 PLA, Injection
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Properties: PLLA

General Properties: PLA is a thermoplastic polyester produced using annually renewable biomass like corn, sugar beet, or sugarcane. Depending on the geographical area of production, the resources used may be certified GMO free.

Applications:
Process:

  • Injection molding and blowing
  • Thermoforming
  • Flat extrusion die or cast
  • Extrusion of profiles
Markets:
  • Rigid packaging: containers, trays, bottles
  • Flexible packaging: film
  • Regular consumption goods
  • Non-woven or textile fiber
Properties:
  • 100% biobased Biodegradable and industrially compostable
  • Rigid and brittle
  • Transparent
  • Food safe

Information provided by NaturePlast Bioplastics Experts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 5.0 %5.0 %ISO 527
Tensile Modulus 3.50 GPa508 ksiISO 527
Charpy Impact Unnotched 2.30 J/cm²10.9 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 51.0 °C124 °FISO 75-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNATPLAS002 / 285451

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.