MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ELM® SoyLube® All Purpose Lubricant and Penetrating Oil
Categories: Fluid; Lubricant

Material Notes: Description: SoyLube All Purpose Lubricant and Penetrating Oil is a high performance, biodegradable penetrant and lubricating oil for general purpose use. Formulated with the best optimized USA-grown natural seed oils and select additives, it surpasses the lubricity and performance of conventional lubricants.

Applications:

  • Multipurpose lubricant and penetrant
  • Loosens rusty bolts
  • Quiets squeaky hinges and moving parts
  • Deters water
  • Protects from rust and corrosion
  • General purpose cutting, grinding and drilling metals
  • Milling, tapping, and reaming
Benefits:
  • Made from plant oils, better for your health
  • Multiple application - Reduces product inventory
  • Superior lubricity improves productivity
  • Cooler operating and less smoke
  • Safe for all metals
  • Will help your business comply with ISO-14000
  • Does not contain chlorine
  • High flash and fire points
  • Made from renewable USA-grown crop-based vegetable oils – Reduces foreign oil dependence.

Information provided by ELM®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Kinematic Viscosity at 40°C (104°F) 40 cSt40 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 8.5 cSt8.5 cStASTM D445
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)ASTM D2596
Four Ball Wear 0.350 mm0.0138 inASTM D4172
 
Thermal PropertiesMetricEnglishComments
Pour Point -20.0 °C-4.00 °FASTM D97
Flash Point 310 °C590 °FASTM D92
 
Descriptive Properties
AppearanceLight Yellow
Pin & Vee Block TestASTM D3233A3335 lbs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WELML026 / 146229

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.