MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Evonik VESTODUR® GF10 Polybutylene Terephthalate  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: Glass fiber-reinforced polybutylene terephthalate compound. VESTODUR® GF10 natural color is a glass fiber-reinforced (10%), semicrystalline, thermoplastic resin based on polybutylene terephthalate (PBT). VESTODUR® GF10 natural color is suitable for the injection molding of parts with high mechanical and thermal resistance. The compound is supplied as cylindrical pellets in polyethylene packaging. Pigmentation may affect values.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ISO 1183
Water Absorption 0.50 %0.50 %Sim. to ISO 62
Moisture Absorption 0.100 %0.100 %Sim. to ISO 62
Linear Mold Shrinkage 0.016 cm/cm0.016 in/inNominal; ISO 294-4, 2577
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4, 2577
Melt Flow 23 g/10 min
@Load 2.16 kg,
Temperature 250 °C
23 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 81
@Time 3.00 sec
81
@Time 0.000833 hour
ISO 7619-1
Ball Indentation Hardness 170 MPa24700 psiISO 2039-1
Tensile Strength at Break 100 MPa14500 psiISO 527
Elongation at Break 4.2 %4.2 %Nominal; ISO 527
Tensile Modulus 4.90 GPa711 ksiISO 527
Charpy Impact Unnotched 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
Complete Break; ISO 179/1eA
 0.550 J/cm²
@Temperature 23.0 °C
2.62 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eA
Tensile Impact Strength 40.0 kJ/m²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
Notched.; ISO 8256/1
Tensile Creep Modulus, 1 hour 4600 MPa
@Strain 0.5 %
667000 psi
@Strain 0.5 %
ISO 899-1
Tensile Creep Modulus, 1000 hours 3100 MPa
@Strain 0.5 %
450000 psi
@Strain 0.5 %
ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+13 ohm1.00e+13 ohmRSD; IEC 62631-3-1
 1.00e+14 ohm1.00e+14 ohmsE; IEC 62631-3-1
Dielectric Constant  3.6
@Frequency 100 Hz
3.6
@Frequency 100 Hz
IEC 62631-2-1
 3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
IEC 62631-2-1
Dielectric Strength 27.0 kV/mm686 kV/inAC, S20/P50; Sim. to IEC 60243-1
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 62631-2-1
 0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 300 V300 Vtest solution A, 100 drops value; IEC 60112
 325 V325 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 223 °C433 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FISO 75-1/-2
Vicat Softening Point 205 °C401 °FMethod B: 10 N, 50 K/h; ISO 306
 220 °C428 °FMethod A: 10 N, 50 K/h; ISO 306
Glass Transition Temp, Tg 45.0 °C113 °FISO 11357-1/-2
Flammability Test  1.0
@Thickness 0.800 mm
1.0
@Thickness 0.0315 in
IEC 60695-11-10
 1.0
@Thickness 1.60 mm
1.0
@Thickness 0.0630 in
IEC 60695-11-10
Glow Wire Ignition Temperature 750 °C
@Thickness 2.00 mm
1380 °F
@Thickness 0.0787 in
Glow Wire Flammability Index 750 °C
@Thickness 2.00 mm
1380 °F
@Thickness 0.0787 in
 
Processing PropertiesMetricEnglishComments
Mold Temperature 80.0 °C176 °FTest condition for mold shrinkage

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical Lupox® GP2100 PBT+GF10%
LG Chemical Lupox® TE5100 PBT+PC+GF10%
BLUESTAR PBT 6630 30% Glass Filled
BASF Ultradur® B 4040 G10 BK5110 50% Glass Filled PBT
Plastcom SLOVASTER® B GF 10 Polybutylene Terephthalate, 10% Glass Fiber

PEVONIK880 / 243087

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.