Unplasticized molding compound based on acrylate-modified suspension PVC for high-impact white window profile for temperate climates. Also for other high-impact, weather-resistant profile. This product is VC/AK modified and Ca/Zn stabilized. Data was collected by ISO methods and provided by BASF. BASF no longer produces PVC products. Their PVC product line is now a part of SolVin, a joint venture with Solvay. |