MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Bada BADAMID® PA12 H UV natural PA12, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Unreinforced, heat- and UV-stabilized polyamide 12 with very good processability in injection molding

Information provided by Bada

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Moisture Absorption 0.700 %0.700 %50% r.h.; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 47.0 MPa6820 psi50 mm/min; ISO 527-1/2
Elongation at Yield 4.0 %4.0 %50 mm/min; ISO 527-1/2
 >= 200 %>= 200 %Nominal, 50 mm/min; ISO 527-1/2
Tensile Modulus 1.70 GPa247 ksi1 mm/min; ISO 527-1/2
Flexural Strength 60.0 MPa8700 psiISO 178
Flexural Modulus 1.50 GPa218 ksiISO 178
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC-62631-3-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 130 µm/m-°C72.2 µin/in-°FISO 11359-2
Melting Point 178 °C352 °F10 K/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-1/2
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Glow Wire Flammability Index  650 °C
@Thickness 0.750 mm
1200 °F
@Thickness 0.0295 in
IEC-60695-2-12
 650 °C
@Thickness 1.50 mm
1200 °F
@Thickness 0.0591 in
IEC-60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 260 °C428 - 500 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.15 %<= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBADA172 / 287005

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.