MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay REPEL-O-TEX® SF2 Surfactant
Categories: Fluid

Material Notes: Description: High active soil release polymer for powder laundry. Prevents adhesion of soils between washes and soil redeposition during wash. Repel-O-Tex SF2 has been specifically formulated for improved flowability and lower dust, providing ease of handling. The high, 96%, active level also improves cost-in-use versus 90% active Repel-O-Tex SF. Both Repel-O-Tex SF and SF2 are salt free versions of Repelotex PF 594.

Chemical Name: SOIL RELEASE POLYMER

Recommended inclusion rate: 0.5 to 1%.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Repel-O-Tex SF2, designed for powder and tablet laundry, imparts soil release properties to polyester fabrics, offering protection against adhesion of greasy soils between wash cycles. Repel-O-Tex SF2 has been specifically formulated for improved flowability and lower dust, providing ease of handling. The high, 96%, active level also improves cost-in-use versus Repel-O-Tex SF. Both Repel-O-Tex SF and SF2 are salt free versions of Repel- O-Tex PF 594.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.650 - 0.850 g/ccRP-0155
Particle Size <= 177 µmThru #100 Mesh; RP-0499
 <= 1400 µmon #35 Mesh; RP-0499
pH 3.0 - 6.01% Dispersion in Water; RP-0420
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 2.0 %
@Temperature 105 °C,
Time 3600 sec
RP-0540
 
Descriptive Properties
AppearanceOff white, Free Flowing PowderRP-0064
CompositionDioxan (1,4)<150 ppm, RP-1412
 Flow aid2-6%, RP-1463
 Polymer94-98%, RP-1463
Dynamic flow rate>35 ml/secRP-8037
Shake Foam Test<23%
 <5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD328 / 137559

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.