MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nouryon Armeen M2HP
Categories: Other Engineering Material

Material Notes: Armeen M2HP is a di(C16/C18 alkyl) methylamine.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.797 g/cc
@Temperature 70.0 °C
0.0288 lb/in³
@Temperature 158 °F
 0.803 g/cc
@Temperature 60.0 °C
0.0290 lb/in³
@Temperature 140 °F
 0.808 g/cc
@Temperature 38.0 °C
0.0292 lb/in³
@Temperature 100 °F
 0.813 g/cc
@Temperature 40.0 °C
0.0294 lb/in³
@Temperature 104 °F
Viscosity  83 cP
@Temperature 65.0 °C
83 cP
@Temperature 149 °F
 105 cP
@Temperature 55.0 °C
105 cP
@Temperature 131 °F
 231 cP
@Temperature 45.0 °C
231 cP
@Temperature 113 °F
Vapor Pressure 0.000133322 bar0.0999998 torr
 
Thermal PropertiesMetricEnglishComments
Melting Point 38.0 °C100 °F
Boiling Point 230 - 310 °C
@Pressure 0.0000266645 MPa
446 - 590 °F
@Pressure 0.00386635 psi
Pour Point 41.0 °C106 °F
Flash Point >= 149 °C>= 300 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 0.00 - 1.00.00 - 1.0
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %
 
Descriptive Properties
Amine number103 - 114
AppearanceSolid
Cloud point48°C
Content= 2 %Primary + Secondary Amine
 = 97 %Tertiary Amine
Equivalent mass524 g/eq

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY207 / 285730

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.