MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kolon CC302 Polarizing Plate Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP

Material Notes: Films for polarizer - defect free polyester base. Films used for protective and adhesive coating during the process of manufacturing polarizer which are used in LCD TVs and Monitors.

Corona treatment possible. Used as MLCC base for release. Paintable. Resistant to n-hexane, ethanol, IPA, toluene, and ethyl acetate.

Information provided by Kolon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Seal Strength 218 g/25 mm3M Remove Tape #244
 884 g/25 mmNitto 31B
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 6.59e+8 ohmGrade 1
 2.59e+9 ohmGrade 2
 
Optical PropertiesOriginal ValueComments
Haze 3.92 %Coating Appearance
 
Descriptive Properties
Water Contact Angle92°

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow C759-21NA Polypropylene Impact Copolymer Resin
Kolon CY312 Silicone Release Film
Envalior Arnitel® XG6029 TPC-ET, Extrusion Grade
Envalior Arnitel® XG5855 TPC-ET, Extrusion Grade

PKOKZ810 / 185353

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.