MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Toray AMILAN™ CM3211G35UB1 Nylon 66, 35% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Nylon 66/ reinforced GF35%/Calcium chloride resistance, PA66/PA610-GF35

General Amilan™ Notes: AMILAN™ nylon (polyamide) is a thermoplastic engineering plastic containing an amide group (-CONH-) and it exhibits excellent strength, toughness, heat resistance, and anti-friction wear resistance. A variety of grades designed for various customer needs and applications are available.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³Dry; ISO 1183
Filler Content 35 %35 %Dry
Water Absorption 1.1 %1.1 %In 23°C water
 3.0 %3.0 %In 23°C water, polymer initally dry; ISO 62
 0.40 %
@Time 86400 sec
0.40 %
@Time 24.0 hour
In 23°C water, polymer initally dry; ISO 62
 0.40 %
@Time 86400 sec
0.40 %
@Time 24.0 hour
In 23°C water, polymer initally dry; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in80x80x3mmt. Dry; Toray Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/in80x80x3mmt. Dry; Toray Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9393Dry; ISO 2039-2
Hardness, Rockwell R 120
@Temperature 23.0 °C
120
@Temperature 73.4 °F
Dry; ISO 2039-2
Tensile Strength  120 MPa
@Temperature 80.0 °C
17400 psi
@Temperature 176 °F
Dry; ISO 527-1,2
 195 MPa
@Temperature 23.0 °C
28300 psi
@Temperature 73.4 °F
Dry; ISO 527-1,2
 280 MPa
@Temperature -40.0 °C
40600 psi
@Temperature -40.0 °F
Dry; ISO 527-1,2
Elongation at Break  3.0 %
@Temperature -40.0 °C
3.0 %
@Temperature -40.0 °F
Dry; ISO 527-1,2
 3.0 %
@Temperature 23.0 °C
3.0 %
@Temperature 73.4 °F
Dry; ISO 527-1,2
 5.0 %
@Temperature 80.0 °C
5.0 %
@Temperature 176 °F
Dry; ISO 527-1,2
Flexural Strength  160 MPa
@Temperature 80.0 °C
23200 psi
@Temperature 176 °F
Dry; ISO 178
 290 MPa
@Temperature 23.0 °C
42100 psi
@Temperature 73.4 °F
Dry; ISO 178
 370 MPa
@Temperature -40.0 °C
53700 psi
@Temperature -40.0 °F
Dry; ISO 178
Flexural Modulus  4.80 GPa
@Temperature 80.0 °C
696 ksi
@Temperature 176 °F
Dry; ISO 178
 9.50 GPa
@Temperature 23.0 °C
1380 ksi
@Temperature 73.4 °F
Dry; ISO 178
 11.0 GPa
@Temperature -40.0 °C
1600 ksi
@Temperature -40.0 °F
Dry; ISO 178
Charpy Impact Unnotched  8.90 J/cm²
@Temperature -40.0 °C
42.4 ft-lb/in²
@Temperature -40.0 °F
Dry; ISO 179
 9.45 J/cm²
@Temperature 23.0 °C
45.0 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179
Charpy Impact, Notched  1.00 J/cm²
@Temperature -40.0 °C
4.76 ft-lb/in²
@Temperature -40.0 °F
V-Notched. Dry; ISO 179
 1.35 J/cm²
@Temperature 23.0 °C
6.42 ft-lb/in²
@Temperature 73.4 °F
V-Notched. Dry; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 101300 ohm-cm101300 ohm-cmDry; IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C11.1 - 16.7 µin/in-°FDry; ISO 11359-2
Thermal Conductivity 0.420 W/m-K2.91 BTU-in/hr-ft²-°FDry
Melting Point 265 °C509 °FDry; DSC Method
Deflection Temperature at 0.46 MPa (66 psi) 228 °C442 °FDry; ISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 225 °C437 °FDry; ISO 75-1,2
Flammability, UL94 HBHBDry

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY9161 / 248850

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.