MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene Select GS906072 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: The Petrothene Select series of resins are high performance hexene, linear low density polyethylenes selected by customers for use in blown film applications that require superior strength and toughness. Petrothene Select GS906 has a melt index of 0.6 g/10 min which can contribute to films having very high dart impact as well as excellent melt strength during blown film fabrication.

Availability: North America

Application: Agriculture Film; Bags & Pouches; Can Liners; Film Wrap; Food Packaging Film; Heavy Duty Packaging; Lamination Film; Liner Film; Retail Carryout Bags; Shipping Sacks; Shrink Film

Market: Flexible Packaging

Processing Method: Blown Film

Attribute: Good Melt Strength; High Impact Resistance; Superior Tear Resistance

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9165 g/ccBase Resin; ASTM D1505
 0.9215 g/ccProduct; ASTM D1505
Melt Flow 0.600 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 8000 ppm
Slip Level 1350 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 500 %ASTM D882
Film Elongation at Break, TD 700 %ASTM D882
Secant Modulus, MD 0.186 GPa1% Modulus; ASTM D882
Secant Modulus, TD 0.200 GPa1% Modulus; ASTM D882
Elmendorf Tear Strength MD 450 gASTM D1922
Elmendorf Tear Strength TD 650 gASTM D1922
Dart Drop Test 650 gASTM D1709
Film Tensile Strength at Break, MD 65.5 MPaASTM D882
Film Tensile Strength at Break, TD 48.3 MPaASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9740 / 324675

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.