MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Covestro DESMODUR® TG263 + BAYTEC® XL 1705, 95 A Polyurethane, TDI- PPG
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccDESMODUR® TG263
 1.14 g/cc1.14 g/cc
 1.21 g/cc1.21 g/ccBAYTEC® XL 1705
Viscosity 690 cP690 cPBAYTEC® XL 1705
 1200 cP1200 cPDESMODUR® TG263
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595DIN 53505
 93
@Temperature 80.0 °C
93
@Temperature 176 °F
DIN 53505
 99
@Temperature -5.00 °C
99
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 30.0 MPa4350 psiDIN 53504
Tensile Stress at Strain 6.40 MPa
@Strain 10 %
928 psi
@Strain 10 %
DIN 53504
Elongation at Break 370 %370 %DIN 53504
100% Modulus 15.1 MPa
@Strain 100 %
2190 psi
@Strain 100 %
DIN 53504
200% Modulus 19.2 MPa
@Strain 200 %
2780 psi
@Strain 200 %
DIN 53504
300% Modulus 24.4 MPa
@Strain 300 %
3540 psi
@Strain 300 %
DIN 53504
Resilience 2929[%]; DIN 53512
Tear Strength 50.0 kN/m285 pliwith nick; ISO 34-1
 105 kN/m599 pliwithout nick; ISO 34-1
Abrasion 4545[mm3]; ISO 4649
Compression Set 53 %
@Temperature 70.0 °C,
Time 79200 sec
53 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 30.0 °C86.0 °FBAYTEC® XL 1705
 70.0 °C158 °FDESMODUR® TG263
Mold Temperature 100 °C212 °F
Pot Life 2.167 min2.167 min
 
Descriptive Properties
AppearanceliquidDESMODUR® TG263
 liquidBAYTEC® XL 1705
Content100Parts by weight of prepolymer
 15.1Parts by weight of BAYTEC® XL 1705
 6.05-6.45%NCO, DESMODUR® TG263

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0618 / 202401

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.