MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Pressure Seal 4525 Chloroprene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 4525 is 50 durometer white colored Chloroprene elastomer, it is formulated with FDA sanctioned materials. It exhibits good physical properties.

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4949
 23
@Treatment Temp. 100 °C,
Time 252000 sec
23
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #3
 26
@Treatment Temp. 23.0 °C,
Time 252000 sec
26
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 40
@Treatment Temp. 100 °C,
Time 252000 sec
40
@Treatment Temp. 212 °F,
Time 70.0 hour
Distilled water aged
 40
@Treatment Temp. 23.0 °C,
Time 252000 sec
40
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
 45
@Treatment Temp. 100 °C,
Time 252000 sec
45
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #1
 55
@Treatment Temp. 100 °C,
Time 252000 sec
55
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
 59
@Treatment Temp. 125 °C,
Time 252000 sec
59
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
Tensile Strength 13.02 MPa1889 psi
 7.2802 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
1055.9 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 7.3719 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
1069.2 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #3
 10.523 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
1526.3 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
 13.402 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
1943.8 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #1
 13.975 MPa
@Treatment Temp. 125 °C,
Time 252000 sec
2026.9 psi
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
 16.554 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
2400.9 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
Elongation, Ultimate 1170 %1170 %
 849.4 %
@Treatment Temp. 125 °C,
Time 252000 sec
849.4 %
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
 859.95 %
@Treatment Temp. 100 °C,
Time 252000 sec
859.95 %
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #3
 910.3 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
910.3 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 980.5 %
@Treatment Temp. 100 °C,
Time 252000 sec
980.5 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
 1009.7 %
@Treatment Temp. 100 °C,
Time 252000 sec
1009.7 %
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #1
 1049.5 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
1049.5 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
100% Modulus 0.765 MPa111 psi
Tear Strength 32.1 kN/m183 pliDie C
 33.5 kN/m191 pliDie B
Compression Set  45.6 %
@Treatment Temp. 100 °C,
Time 79200 sec
45.6 %
@Treatment Temp. 212 °F,
Time 22.0 hour
Solid
 56.7 %
@Treatment Temp. 100 °C,
Time 252000 sec
56.7 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Solid
 64 %
@Treatment Temp. 100 °C,
Time 79200 sec
64 %
@Treatment Temp. 212 °F,
Time 22.0 hour
Plied
 70.3 %
@Treatment Temp. 100 °C,
Time 252000 sec
70.3 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Plied
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -44.4 °C-48.0 °F
Shrinkage  6.7 %
@Treatment Temp. 100 °C,
Time 252000 sec
6.7 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, ASTM Oil #1
 21.7 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
21.7 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel A
 64.6 %
@Treatment Temp. 100 °C,
Time 252000 sec
64.6 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, Distilled water aged
 89.6 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
89.6 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel B
 142.4 %
@Treatment Temp. 100 °C,
Time 252000 sec
142.4 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, ASTM Oil #3
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRESL068 / 318278

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.