MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChevronTexaco Delo® ESI® Trans Fluid
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Delo Trans Fluid ESI is a premium grade, heavy duty truck manual transmission fluid formulated with ISOSYN™ base stocks and compounded with a unique extreme pressure additive utilizing an inorganic borate compound. It also contains oxidation, corrosion, rust, and foam inhibitors. This product is ideally suited for transmissions exposed to extremely high temperatures and loads.

Applications

Chevron Delo Trans Fluid ESI is recommended for use in heavy duty manual transmissions. Its outstanding low temperature flow properties and high viscosity index provides superior all-climate, year-round performance in heavy duty truck transmissions. Its use permits easie shifting in cold weather and less wear during startup as well as providing for potential fuel economy.

Its exceptional thermal and oxidation stability, and antiwear performance, permit longer transmission life and extended drain intervals.

Chevron Delo Trans Fluid ESI is the only nonsynthetic transmission fluid approved for Eatons 750,000 mile extended warranty program (Eaton PS-081)

Key Words: CPS Number: 235062; MSDS Number: 6976
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 28.2 °28.2 °
Viscosity Measurement 9999Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 754 SUS754 SUS
Saybolt Viscosity at 210°F 78 SUS78 SUS
Kinematic Viscosity at 40°C (104°F) 143.8 cSt143.8 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 14.5 cSt14.5 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -33.0 °C-27.4 °FASTM D97
Flash Point 210 °C410 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCHEV043 / 74658

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.