Produced without animal derived components Sterilization: Gamma radiation, EtO, E-beam, and autoclave Applications: Medical bottles, syringes, centrifuge tubes Regulatory: FDA – 21 CFR 177.1520(c) 3.2a; USP <88> Class VI, USP<85>, and ISO 10993-5 Information provided by INVISTA. |