MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF ε-Caprolactone
Categories: Fluid

Material Notes: Formula: C6H10O2

CAS: 502-44-3

Description: Epsilon-caprolactone is a colorless to yellow liquid, with a perceptible odor. It is soluble in water.

Synonyms: 6-Hydroxyhexanoic acid lactone, Caprolacton, 6-Hexanolide

Applications: Intermediate used in the production of Adhesives, Modifier in resins and polymers, Paints, Polycaprolactone and TPU

Information provided by BASF

Key Words: Epsilon-Caprolactone
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.078 g/cc0.03895 lb/in³
Molecular Weight 114.1 g/mol114.1 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point <= -1.50 °C<= 29.3 °F
Boiling Point 96.0 - 97.0 °C205 - 207 °F
Flash Point 127 °C261 °F
Ignition Temperature 204 °C399 °F
 
Descriptive Properties
Assay>99.8%
Color<15APHA, DIN EN 1557

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BiologiQ EcoStarch GS270 Thermoplastic Starch
Covestro DESMODUR® ML3182 + BAYTEC® XL AL905 (SD11-3) 90 A Polyurethane, MDI- Caprolactone
Covestro DESMODUR® MLQ22165 + BAYTEC® L20 + BAYTEC® XL B (Catalyst SD11-2) 75 A Polyurethane, MDI- Caprolactone
Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane
BASF Dicykan 4,4'-Diaminodicyclohexylmethane

PBASG0936 / 132569

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.