MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Manganese Brass, Copper Alloy, UNS C66900, H02 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: 1/2 Hard

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.11 g/cc0.293 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7979
Hardness, Rockwell 30T 7171
Tensile Strength 503 MPa73000 psi
Tensile Strength, Yield 414 MPa60000 psi0.2% Offset
Elongation at Break 16 %16 %
Tensile Modulus 110 GPa16000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000510 ohm-cm0.0000510 ohm-cm3.4% IACS
 
Thermal PropertiesMetricEnglishComments
Melting Point 845.0 - 858.3 °C1553 - 1577 °F
Solidus 845.0 °C1553 °F
Liquidus 858.3 °C1577 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 62.5 - 64.5 %62.5 - 64.5 %
Iron, Fe <= 0.25 %<= 0.25 %
Lead, Pb <= 0.050 %<= 0.050 %
Manganese, Mn 11.5 - 12.5 %11.5 - 12.5 %
Zinc, Zn 23 - 26 %23 - 26 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC66900x1 / 292291

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.