MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestamid® L-GF30 30% Glass Filled Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: Description: 30% chopped strands, medium-viscosity, heat-stabilized, with processing aid

Applications: Bearing cups for windshield wipers

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA12,MHR,18-070,GF30
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccISO 1183
Moisture Absorption at Equilibrium 0.50 %
@Thickness 1.00 mm,
Temperature 23.0 °C
50% R.H.; ISO 62
Water Absorption at Saturation 1.1 %
@Thickness 1.00 mm
ISO 62
Linear Mold Shrinkage 0.0030 cm/cm127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse 0.0090 cm/cm127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPaISO 527-1/2
Elongation at Break 5.0 %ISO 527-1/2
Tensile Modulus 6.50 GPaISO 527-1/2
Charpy Impact Unnotched 8.50 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
 10.0 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 2.10 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 2.30 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.4
@Frequency 1e+6 Hz
IEC 60250
 4.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 44.0 kV/mmK20/P50; IEC 60243-1
Dissipation Factor 0.031
@Frequency 100 Hz
IEC 60250
 0.033
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 VTest Solution A, 50 drops; IEC 60112
 600 VTest Solution A, 100 drops; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
45x15x10 mm; ISO 11359
Melting Point 178 °CPeak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 175 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 165 °CISO 75
Vicat Softening Point 175 °C10N; ISO 306
 175 °C50N; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
 
Descriptive Properties
ColorBlack
Electrolytic CorrosionA1 StepIEC 60426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestamid® L1833 30% Glass Filled Nylon 12
Kingfa PA66-G30 30% Glass Fiber Reinforced PA66
Evonik Vestamid® L-GF15 23% Glass Filled Nylon 12
Evonik Vestamid® L-CF15 sw 15% Carbon Fiber Reinforced, Antistatic, Black, Electrically Conductive Nylon 12
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned)

PHULA46 / 47406

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.