MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
GEHR Plastics PA 6.6 Nylon 6.6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccISO 1183
Water Absorption 8.0 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.0 MPaISO 527
Elongation at Yield >= 100 %ISO 527
Modulus of Elasticity 1.65 GPaISO 527
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+12 ohm-cmVDE 0303
Surface Resistivity per Square >= 1.00e+12 ohmVDE 0303
Dielectric Constant 3.8
@Frequency 1e+6 Hz
DIN 53483
Dielectric Strength 18.0 kV/mmVDE 0303
Dielectric Loss Index 0.060
@Frequency 1e+6 Hz
DIN 53483
 
Descriptive Properties
Aromatic Resistancelimited
ColorNatural
Hydrocarbonate Resistancelimited
Ketone Resistancelimited
Resistance Against Hot Waterlimited

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GEHR Plastics PA 6.6 Nylon 6.6, Dry
GEHR Plastics PA 6.6-30GF Nylon 6.6, 30% Glass Fiber, Dry
Iran Petrochemical (PCC) PC 0104 Polycarbonate
LATI Latamid 66 H2 K/20 PA 66, 20% Carbon Fiber Reinforced, Heat Stabilized
GEHR Plastics PC Polycarbonate

PGEHR019 / 79856

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.