MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tin Bronze, UNS C91300, Copper Casting Alloy, M07 Temper, As Continuous Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Continuous Cast

Casting Characteristics: High – Fluidity; Medium – Effect of Section Size, Casting Yield; Med-High – Gassing; Low - Drossing, Shrinkage in Solidification

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability - Brazing; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding

Typical uses: Bells; Bearings; Bushings; Piston Rings; Valve Bodies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 16000 ksi
Machinability 10 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000250 ohm-cm7% IACS
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.0900 BTU/lb-°F
Melting Point 1505 - 1632 °F
Solidus 1505 °F
Liquidus 1632 °F
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 500 °FStress Relief
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb <= 0.20 %
Copper, Cu 79 - 82 %
Iron, Fe <= 0.25 %
Lead, Pb <= 0.25 %
Nickel, Ni <= 0.50 %
Phosphorus, P <= 1.0 %
Silicon, Si <= 0.0050 %
Sulfur, S <= 0.050 %
Tin, Sn 18 - 20 %
Zinc, Zn <= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC91300x1 / 293199

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.