MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for 6000 Series Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "6000 Series Aluminum Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.68 - 2.92 g/ccAverage value: 2.71 g/cc Grade Count:191
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 25.0 - 130Average value: 89.7 Grade Count:77
Hardness, Knoop 73.0 - 163Average value: 121 Grade Count:47
Hardness, Rockwell A 35.5 - 49.5Average value: 43.0 Grade Count:33
Hardness, Rockwell B 49.0 - 88.0Average value: 67.6 Grade Count:39
Hardness, Vickers 35.0 - 149Average value: 106 Grade Count:49
Tensile Strength, Ultimate 89.6 - 565 MPaAverage value: 334 MPa Grade Count:103
Tensile Strength, Yield 40.0 - 517 MPaAverage value: 283 MPa Grade Count:103
Elongation at Break 1.00 - 35.0 %Average value: 11.0 % Grade Count:99
Modulus of Elasticity 67.0 - 140 GPaAverage value: 83.2 GPa Grade Count:83
Compressive Yield Strength 365 - 490 MPaAverage value: 423 MPa Grade Count:3
Compressive Modulus 96.0 - 121 GPaAverage value: 107 GPa Grade Count:3
Ultimate Bearing Strength 228 - 1080 MPaAverage value: 830 MPa Grade Count:6
Bearing Yield Strength 103 - 1100 MPaAverage value: 749 MPa Grade Count:6
Poissons Ratio 0.296 - 0.330Average value: 0.327 Grade Count:54
Fatigue Strength 55.0 - 517 MPaAverage value: 170 MPa Grade Count:32
Machinability 30.0 - 90.0 %Average value: 64.6 % Grade Count:26
Shear Modulus 25.8 - 53.8 GPaAverage value: 28.1 GPa Grade Count:53
Shear Strength 60.0 - 331 MPaAverage value: 204 MPa Grade Count:74
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000280 - 0.00000500 ohm-cmAverage value: 0.00000384 ohm-cm Grade Count:94
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.1 - 25.6 µm/m-°CAverage value: 23.0 µm/m-°C Grade Count:99
Specific Heat Capacity 0.800 - 0.900 J/g-°CAverage value: 0.886 J/g-°C Grade Count:53
Thermal Conductivity 130 - 226 W/m-KAverage value: 178 W/m-K Grade Count:90
Melting Point 554 - 655 °CAverage value: 620 °C Grade Count:71
Solidus 554 - 621 °CAverage value: 593 °C Grade Count:71
Liquidus 645 - 655 °CAverage value: 651 °C Grade Count:67
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 349 - 546 °CAverage value: 411 °C Grade Count:39
Solution Temperature 504 - 566 °CAverage value: 525 °C Grade Count:63
Aging Temperature 149 - 204 °CAverage value: 172 °C Grade Count:59
Hot-Working Temperature 260 - 510 °CAverage value: 380 °C Grade Count:12
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 91.7 - 99.6 %Average value: 97.0 % Grade Count:191
Bismuth, Bi 0.150 - 1.50 %Average value: 0.644 % Grade Count:27
Boron, B 0.00300 - 0.0600 %Average value: 0.0543 % Grade Count:10
Chromium, Cr 0.0300 - 0.400 %Average value: 0.154 % Grade Count:165
Copper, Cu 0.0100 - 1.20 %Average value: 0.323 % Grade Count:191
Cr + Mn 0.120 - 0.500 %Average value: 0.323 % Grade Count:3
Iron, Fe 0.0400 - 1.00 %Average value: 0.472 % Grade Count:190
Lead, Pb 0.00300 - 2.00 %Average value: 0.325 % Grade Count:21
Magnesium, Mg 0.200 - 3.00 %Average value: 0.836 % Grade Count:191
Manganese, Mn 0.0200 - 1.40 %Average value: 0.281 % Grade Count:178
Nickel, Ni 0.0500 - 0.200 %Average value: 0.100 % Grade Count:3
Oxygen, O 0.0500 - 0.500 %Average value: 0.275 % Grade Count:9
Silicon, Si 0.200 - 1.80 %Average value: 0.730 % Grade Count:187
Strontium, Sr 0.0500 %Average value: 0.0500 % Grade Count:8
Tin, Sn 0.0500 - 2.00 %Average value: 0.850 % Grade Count:19
Titanium, Ti 0.0100 - 0.250 %Average value: 0.131 % Grade Count:154
Vanadium, V 0.0500 - 0.300 %Average value: 0.148 % Grade Count:16
Zinc, Zn 0.0300 - 2.40 %Average value: 0.217 % Grade Count:183
Zirconium, Zr 0.0500 - 0.200 %Average value: 0.109 % Grade Count:7
Zr+Ti 0.150 - 0.200 %Average value: 0.183 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for 5000 Series Aluminum Alloy
Overview of materials for 7000 Series Aluminum Alloy
Overview of materials for 2000 Series Aluminum Alloy
Overview of materials for 3000 Series Aluminum Alloy
Overview of materials for 4000 Series Aluminum Alloy

M01045 / 81687

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.