Standard straight novolak type powder Applications: Brake Lining and Disc Pad SUMILITERESIN® PR-1012 AI is a powder phenolic resin with good friction properties and other merits in friction production. SUMILITERESIN® PR-1012 AI has a short gel time and very fine particle size. It has a high reactive resin and fast cure. It is effective to reduce hot process and post cure time. SUMILITERESIN® PR-1012 AI has a hexamine content of approximately 9% and a medium molecular weight. By theses properties, it will be suitable to apply in brake lining and disc pad with good hardness and bending strength. Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |