MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Avient Nymax™ 1108 UV Natural Nylon 6  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of fillers, glass reinforcement levels, and impact modifiers depending upon grade selected and have been formulated to offer ease of processing in most standard thermoplastic processing equipment.

Property data measured on molded test bars: Dry as Molded

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
Water Absorption 1.5 %
@Thickness 3.18 mm,
Time 86400 sec
1.5 %
@Thickness 0.125 in,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.012 - 0.014 cm/cm0.012 - 0.014 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 62.7 MPa9090 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 65 %65 %Type I, 5.1 mm/min; ASTM D638
Flexural Strength 82.7 MPa12000 psiASTM D790
Flexural Modulus 2.24 GPa325 ksiASTM D790
Izod Impact, Notched 0.961 J/cm
@Thickness 3.18 mm
1.80 ft-lb/in
@Thickness 0.125 in
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
@Thickness 3.18 mm
129 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 
Descriptive Properties
AdditiveImpact Modifier
 UV Stabilizer
AppearanceNatural Color
FeaturesGeneral Purpose
 Impact Modified
FormsPellets
Generic NamePolyamide 6 (Nylon 6)
Processing MethodInjection Molding
Regional AvailabilityNorth America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PH1PN9248 / 103084

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.