MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Oppalyte™ 30MD447 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for use on VFFS and HFFS machines and is also very well suited for overwrapping applications.

Availability: Africa & Middle East, Asia Pacific and Europe

Key Features:

  • Excellent stiffness and flex resistance
  • Good seal strength
  • Excellent dimensional stability
  • Good hot slip
  • Good hot tack
Features:
  • In Lamination Lap Sealable
  • Light Barrier
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Box Overwrap
  • Confectionery, Chocolate
  • Confectionery, Gum
  • Confectionery, Sugar
  • Crisps and Snacks
  • Fresh Produce
  • Frozen Food
  • Health and Beauty Care
  • Household Detergents
  • Ice Cream
  • Pet Food
Uses:
  • Box Overwrap Flexible Packaging
  • HFFS Flexible Packaging
  • Pouches-Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Inner Web Extrusion Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing and Surface Print Unsupported

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brightness 90.0 %90.0 %Whiteness Index
Water Vapor Transmission  1.10 g/m²/day
@Temperature 23.0 °C
0.0710 g/100 in²/day
@Temperature 73.4 °F
85% RH; ExxonMobil Method
 4.97 g/m²/day
@Temperature 38.0 °C
0.320 g/100 in²/day
@Temperature 100 °F
90% RH; ExxonMobil Method
Thickness 30.5 microns1.20 milExxonMobil Method
Coating Weight 23.5 g/m²14.7 lb/reamExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 160 %160 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 65 %65 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 1.70 GPa247 ksiMD; ExxonMobil Method
 3.20 GPa464 ksiTD; ExxonMobil Method
Coefficient of Friction 0.250.25Untreated Surface; ExxonMobil Method
 0.300.30Treated Surface; ExxonMobil Method
Seal Strength 410 g/25 mm
@Pressure 0.276 MPa,
Temperature 140 °C
410 g/in
@Pressure 40.0 psi,
Temperature 284 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
Film Tensile Strength at Break, MD 120 MPa17400 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 200 MPa29000 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 3.0 %
@Temperature 135 °C,
Time 432 sec
3.0 %
@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Shrinkage, TD 3.0 %
@Temperature 135 °C,
Time 432 sec
3.0 %
@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Gloss 55 %55 %45°; ExxonMobil Method
Transmission, Visible 33 %33 %ExxonMobil Method
 
Descriptive Properties
Heat Seal Range45°FUntreated, 36.3 psi, 0.2 sec
 72°FTreated, 36.3 psi, 0.2 sec
Yield29200 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Hostaphan® RN, 125 micron Nominal Thickness Universal Polyethylene Terephthalate Film
ExxonMobil Metallyte™ 18MM882 OPP Film
ExxonMobil Bicor™ 15MB440 OPP Film

PEX99497 / 175733

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.