MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A. Schulman BMC T45HT Automotive Grade Molding compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: BMC T45HT was designed for the very demanding applications of automotive under hood engine covers. It meets the GMP UP .007 specification for automotive under hood. BMC T45HT is a vinyl ester based molding compound that has exceptional physical properties along with excellent corrosion and heat resistance. Typical uses are valve covers, rocker arm covers and timing chain covers.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.69 - 1.89 g/ccMolded
Linear Mold Shrinkage 0.0010 - 0.0020 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 50 - 60
Tensile Strength 11300 - 13300 psi
Flexural Strength 24300 - 28300 psi
Flexural Modulus 2000 - 2200 ksi
Compressive Strength 27000 - 31000 psi
Izod Impact, Notched 12.7 - 14.7 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 350 - 400 V/milshort time
Arc Resistance 180 sec
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 425 - 500 °F
Flammability, UL94 HBThis product is not currently UL listed.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 290 - 340 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound
A. Schulman BMC T40(18)-LS Die Casting Replacement Grade Molding Compound
A. Schulman BMC T12(18) General Purpose Molding Compound
A. Schulman BMC A50-XHS-U Bulk molding compound
A. Schulman BMC A50-XHS Bulk molding compound

PBMC951 / 123415

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.