Dexflex thermoplastic polyolefins (TPOs) are in use in applications once reserved for more expensive engineering resins. The performance of these TPOs, combined with their quality and consistency, makes them cost-effective alternatives in automotive applications. Dexflex D60-UV YGYA FS is a thermoplastic olefin elastomeric (TPO) typically used for automotive exterior applications that require toughness, low thermal expansion and exceptional weatherability. Applications: Automotive Parts, Exterior Automotive Applications.Information provided by LyondellBasell. |