MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay RHODACAL® LSS-40/A Surfactant
Categories: Fluid

Material Notes: Description: X High-foaming detergent and emulsifier. Alkali stable. Also used as a foam booster, dispersant and wetter in dishwashing, car- wash products and general- purpose cleaners.

Chemical Name: SODIUM ALPHA OLEFIN SULFONATE

CAS: 68439-57-6

Available in: North America

Applications: RHODACAL® LSS-40/A combines excellent detergency properties and foaming properties with high solubility and lower irritancy than sodium alkyl sulfates and sodium alkyl benzene sulfonates. It is recommended for the following: bubble baths, shampoos, fine fabric wash formulation, liquid soaps, and hand dishwash liquids.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
pH 6.5 - 8.56.5 - 8.55% Active; RP-17601
Viscosity 120 cP120 cP
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Fe (Iron) <= 5.0 ppm<= 5.0 ppmRP-17610
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceClear Amber LiquidRP-17620
Color<100KLETT, 5% Active, RP-17604
CompositionActive38-40%, MW 324, RP-17102
 Free Oil<1.5%, RP-17607
 Sodium Chloride<1.2%, RP-17504
 Sodium Sulfate<1.6%, RP-17503

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODACAL® N Surfactant
Solvay RHODACAL® DS-4 Surfactant
Solvay RHODACAL® DSB Surfactant
Solvay RHODACAL® DS-10 Surfactant
Solvay RHODACAL® 70/B Surfactant

WRHOD340 / 137571

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.