0.005 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.029 in + 0.003, -0.000 (0.74 mm + 0.08, -0.00). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Blue. Weight: 983.3 g/m² ± 67.8 (29.0 oz./yd.² ± 2.0). Shelf Life: 6 months from the date of manufacture. Cure Time: 0.25 hours. Post Cure: 204°C (400°F), for 2 hours. Information provided by the manufacturer, Arlon Silicone Technologies Division. Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation. |