MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Gear Shield® Synthetic Gear Lubricant
Categories: Fluid; Lubricant

Material Notes: Phillips 66® Gear Shield Synthetic is a viscous, adhesive, transparent synthetic based gear lubricant cut back with a volatile, non-chlorinated solvent for ease of application. It is recommended primarily for the lubrication and cushioning of open and semi-enclosed gears found on stationary equipment, such as ball and rod mills, kilns and paper mills. Gear Shield Synthetic is specially formulated to provide high load-carrying capacity to protect heavily loaded gears from scoring and galling. It forms a heavy, tenacious film (after solvent evaporation) that adheres well to metal surfaces and will not harden or flake off at low temperatures. This film has good resistance to water washout and protects the gears against rust and corrosion.

Applications:

  • Open and semi-enclosed gears, such as those found on mining ball and rod mills, cement mills, drying kilns, and papermaking machinery and presses
  • Mills used to process minerals such as gold, copper, iron, taconite and Phosphate
  • Guides and sliding surfaces with large clearances, where asphaltic-type lubricants are specified
  • Cables on draglines, clamshells, shovels, hoists and other cable-operated equipment where cable clamp safety devices are not used
Gear Shield Synthetic meets the requirements of the following industry specification:
  • ANSI/AGMA Standard 9005-E02
Features/Benefits:
  • Excellent adhesion to metal surfaces
  • Forms a heavy, tenacious fi lm to lubricate and cushion gear teeth
  • Good extreme-pressure properties for protection under heavy or shock loads
  • Good resistance to water washout
  • Protects against rust and corrosion
  • Will not flake off at low temperatures
  • Drains freely from gear guards
  • Does not contain any chlorine, lead or carcinogens
  • Easy application, by spraying, brushing or dripping(1)
  • Suitable for use with automatic lubrication equipment

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.913 g/cc
Density 7.60 lb/gal
Kinematic Viscosity at 40°C (104°F) 7200 cStwith solvent
 55100 cStwithout solvent
Kinematic Viscosity at 100°C (212°F) 33350 cStwith solvent
 255225 cStwithout solvent
ASTM Color 2.0ASTM D1500
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 128[kg]; ASTM D2596
Four Ball Extreme Pressure, Weld Load 620 kgASTM D2596
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 49.0 °C
Minimum Service Temperature, Air -18.0 °C
Flash Point >= 150 °CCOC, with solvent
 
Descriptive Properties
ColorAmber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5366 / 198619

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.