MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
American Elements Magnesium Oxide Nanopowder
Categories: Ceramic; Oxide; Magnesium Oxide

Material Notes: General Description

Magnesium Oxide Nanoparticles or Magnesia Nanoparticles (MgO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Magnesium Oxide Nanoparticles or Magnesia Particles are typically 5 - 100 nanometers (nm) with specific surface area (SSA) in the 25 – 50 m 2 /g range. Nano Magnesium Oxide Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for magnesium oxide nanocrystals include as an anti-microbial, anti-biotic (biocide) and anti-fungal (fungicide) agent when incorporated in coatings, bandages, nanofiber, nanowire, plastics, alloy and textiles and further research for their potential electrical, optical, imaging, and other biomedical and bioscience properties.

Key Words: Formula: MgO; CAS Number: 1309-48-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.60 g/cc
Particle Size 0.0050 - 0.10 µm
Specific Surface Area 25 - 50 m²/g
Molecular Weight 40.3 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 2830 °C
Boiling Point 3600 °C
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium Oxide, MgO (Periclase)
MarkeTech Magnesium Oxide (MgO) Single Crystal Substrate
MarkeTech Repton 914 Magnesia MgO
MarkeTech Repton EXP 22 Magnesia MgO
Copper, Cu; Annealed

EJAMER53 / 5536

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.