An extruded, 30% glass fiber reinforced grade PEEK with excellent dimensional stability and outstanding chemical, corrosion, and creep resistance.
|
TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.comClick here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |