MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman BMC T15(GP) General Purpose Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is available in all colors and is UL listed.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.83 - 2.03 g/ccMolded
Linear Mold Shrinkage 0.0020 - 0.0030 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 45 - 50
Tensile Strength 8500 - 10500 psi
Flexural Strength 17000 - 21000 psi
Flexural Modulus 1700 - 1800 ksi
Compressive Strength 18600 - 22600 psi
Izod Impact, Notched 5.00 - 7.00 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 335 - 385 V/milshort time
Arc Resistance >= 185 sec
Comparative Tracking Index >= 500 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 500 °F
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Processing Temperature 280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman BMC T15(F) High Strength Grade Molding Compound
Overview of materials for Polyester (Thermoset) - Rigid
A. Schulman BMC T15(GPT) General Purpose Molding Compound
A. Schulman BMC T15(GPS) General Purpose Molding Compound
A. Schulman BMC 5436 Mineral Filled, Glass Reinforced Polyester

PBMC936 / 123400

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.