MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm Plexiglas® 99845 Crystal Clear Elastomer Based Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Acrylic (PMMA); Elastomer, TPE

Material Notes: Description: PLEXIGLAS® Clear Film 99845, based on polymethyl methacrylate and polybutyl acrylate elastomers, is absolutely crystal-clear. The film shows very good weather resistance and offers substrates excellent protection against natural UV radiation, of which it absorbs more than 98 %. Moreover, the film is resistant to stress whitening. The UV absorber is chemically bound and is not susceptible to migration.

Specific Notes for this Material: PLEXIGLAS® Film 99845 is suitable as a UV and weather protection film for colored or grained PVC window profiles and for protecting sheets and profiles made from PVC or glass-reinforced polyester. It offers UV protection for garden furniture with decorative surfacing as well as UV protection and upgrades surfaces for outside doors made of PVC or ABS.

Information provided by degussa.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 45.0 MPano direction given; ISO 527
Film Elongation at Break, MD 25 %no direction given; ISO 527
Film Elongation at Yield, MD 4.0 %no direction given; ISO 527
Tensile Modulus 1.00 GPaISO 527
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmNo thickness given; IEC 250
Surface Resistance >= 1.00e+13 ohmIEC 250
Dissipation Factor 0.030
@Frequency 1e+6 Hz
IEC 250
 0.040
@Frequency 100 Hz
IEC 250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µm/m-°C
@Temperature 0.000 - 50.0 °C
DIN 53752A
Specific Heat Capacity 1.50 J/g-°C
Vicat Softening Point 104 °CISO 306, Method B 50
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ISO 489
Haze <= 1.0 %ASTM D1003
Yellow Index <= 0.40 %ASTM D1925
Transmission, Visible 92 %DIN 5036
UV Transmittance <= 2.5 %DIN 5036
 
Descriptive Properties
Pencil Hardness3H-4HASTM D3363

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucite International Elvacite® 2044 Acrylic Resin
Polycasa Acryl® KR 2007/1 Acrylic
Polycasa Acryl® KR 2014/1 Acrylic, Impact Grade
Röhm PLEXIGLAS® Film HC 0F028 PMMA
Shinil Chemical SHINCON PMMA Electro Conductive Polymer

PHUK019 / 47153

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.