MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger DELRIN® 507 Black Acetal Homopolymer (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: Delrin® 507 is a general purpose homopolymer acetal containing a UV stabilizer ideally suited for outdoor applications or those in which there is an otherwise abundant source of UV light.
  • General higher surface hardness
  • Easily machinable
  • Designed for outdoor applications
Delrin 507 Black is typically used for outdoor applications in such industries as electronics, communications, transportation, construction and marine.

Information provided by Ensinger

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Water Absorption 0.20 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 91ASTM D785
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Yield 10240 psiASTM D638
Elongation at Break 10 %ASTM D638
Tensile Modulus 366 ksiASTM D638
Flexural Strength 19400 psiASTM D790
Flexural Modulus 482 ksiASTM D790
Izod Impact, Notched 1.28 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 347 °FASTM D3418
Maximum Service Temperature, Air 200 °Flong term; ASTM D648
Deflection Temperature at 0.46 MPa (66 psi) 336 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 237 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Delrin® 150 Homopolymer Acetal (POM)
Delrin Delrin® 100 NC010 POM
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM)
Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM)
Delrin Delrin® 100 BK602 POM

PENSIN091 / 122201

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.