Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.19 g/cc | 1.19 g/cc |
Density | 1.20 g/cc | 0.0434 lb/in³ |
Moisture Absorption | 0.110 % @Temperature 23.0 °C | 0.110 % @Temperature 73.4 °F |
Water Absorption at Saturation | 0.14 % @Temperature 23.0 °C | 0.14 % @Temperature 73.4 °F |
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm | 0.0055 - 0.0075 in/in @Thickness 0.126 in |
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm | 0.0060 - 0.0080 in/in @Thickness 0.126 in |
Melt Flow | 5.0 g/10 min @Load 1.20 kg, Temperature 300 °C | 5.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
| 5.0 g/10 min @Load 1.20 kg, Temperature 300 °C | 5.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 52.0 MPa | 7540 psi |
| 52.0 MPa | 7540 psi |
Tensile Strength, Yield | 67.0 MPa | 9720 psi |
| 68.0 MPa | 9860 psi |
Elongation at Break | 23 % | 23 % |
| 51 % | 51 % |
Elongation at Yield | 6.0 % | 6.0 % |
| 6.0 % | 6.0 % |
Tensile Modulus | 2.40 GPa | 348 ksi |
| 2.50 GPa | 363 ksi |
Flexural Yield Strength | 103 MPa | 14900 psi |
| 106 MPa | 15400 psi |
Flexural Modulus | 2.40 GPa | 348 ksi |
| 2.50 GPa | 363 ksi |
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C | 1.59 ft-lb/in @Temperature -22.0 °F |
| 1.00 J/cm @Temperature 23.0 °C | 1.87 ft-lb/in @Temperature 73.4 °F |
Izod Impact, Unnotched | NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
| NB @Temperature 23.0 °C | NB @Temperature 73.4 °F |
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C | 4.28 ft-lb/in² @Temperature -22.0 °F |
| 10.0 kJ/m² @Temperature 23.0 °C | 4.76 ft-lb/in² @Temperature 73.4 °F |
Izod Impact, Unnotched (ISO) | NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
| NB @Temperature 23.0 °C | NB @Temperature 73.4 °F |
Charpy Impact Unnotched | NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
| NB @Temperature 23.0 °C | NB @Temperature 73.4 °F |
Charpy Impact, Notched | 0.900 J/cm² @Temperature -30.0 °C | 4.28 ft-lb/in² @Temperature -22.0 °F |
| 1.00 J/cm² @Temperature 23.0 °C | 4.76 ft-lb/in² @Temperature 73.4 °F |
Instrumented Impact Total Energy | 66.0 J @Temperature 23.0 °C | 48.7 ft-lb @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Dielectric Constant | 2.79 @Frequency 1.10e+9 Hz | 2.79 @Frequency 1.10e+9 Hz |
Dissipation Factor | 0.0058 @Frequency 1.10e+9 Hz | 0.0058 @Frequency 1.10e+9 Hz |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C | 36.7 µin/in-°F @Temperature -40.0 - 104 °F |
| 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C | 40.0 µin/in-°F @Temperature 73.4 - 176 °F |
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C | 38.9 µin/in-°F @Temperature -40.0 - 104 °F |
| 76.0 µm/m-°C @Temperature 23.0 - 80.0 °C | 42.2 µin/in-°F @Temperature 73.4 - 176 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 131 °C | 268 °F |
| 131 °C @Thickness 3.20 mm | 268 °F @Thickness 0.126 in |
Deflection Temperature at 1.8 MPa (264 psi) | 120 °C | 248 °F |
| 120 °C @Thickness 3.20 mm | 248 °F @Thickness 0.126 in |
Vicat Softening Point | 136 °C | 277 °F |
| 137 °C | 279 °F |
| 139 °C | 282 °F |
UL RTI, Electrical | 125 °C | 257 °F |
UL RTI, Mechanical with Impact | 120 °C | 248 °F |
UL RTI, Mechanical without Impact | 125 °C | 257 °F |
Flammability, UL94 | V-2 @Thickness 0.400 mm | V-2 @Thickness 0.0157 in |
| V-0 @Thickness 1.00 mm | V-0 @Thickness 0.0394 in |
| 5VA @Thickness 3.00 mm | 5VA @Thickness 0.118 in |
Oxygen Index | 45 % | 45 % |
Glow Wire Ignition Temperature | 875 °C @Thickness 1.00 mm | 1610 °F @Thickness 0.0394 in |
Glow Wire Flammability Index | 960 °C @Thickness 1.00 mm | 1760 °F @Thickness 0.0394 in |
|
Optical Properties | Metric | English | Comments |
---|
Transmission, Visible | >= 91 % | >= 91 % |
|
Descriptive Properties |
---|
UV-light, water exposure/immersion | F1 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding