MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Technetium, Tc; Annealed
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: Annealed applies only to tensile and/or hardness values; other property values are typical of the element. Property values for Tc-99. Annealed 10 min at 950°C (1740°F)

See also As-Rolled Tc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 11.5 g/cc0.415 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 9898Longest-Lived Isotope (1995)
Atomic Number 4343
X-ray Absorption Edge 0.58888 Å0.58888 ÅK
 4.06426 Å4.06426 ÅLI
 4.42714 Å4.42714 ÅLII
 4.62537 Å4.62537 ÅLIII
Electronegativity 2.12.1Pauling
Ionic Radius 0.979 Å0.979 ÅCrystal Ionic Radius for Valence +7
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 112112
Hardness, Vickers 151151
Tensile Strength, Ultimate 800 MPa116000 psi
Tensile Strength, Yield 320 MPa
@Strain 0.2 %
46400 psi
@Strain 0.2 %
Elongation at Break 30 %30 %in 25 mm
Tensile Modulus 322 GPa46700 ksi
Bulk Modulus 281 GPa40800 ksi
Poissons Ratio 0.310.31
Shear Modulus 123 GPa17800 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000185 ohm-cm0.0000185 ohm-cm
Magnetic Susceptibility 0.00000270.0000027cgs/g
Critical Magnetic Field Strength, Oersted 14101410
Critical Superconducting Temperature 7.80 K7.80 K
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.05 µm/m-°C
@Temperature -120 - 25.0 °C
3.92 µin/in-°F
@Temperature -184 - 77.0 °F
Thermal Conductivity 50.6 W/m-K351 BTU-in/hr-ft²-°FPolycrystalline Sample
Melting Point 2200 °C3990 °F
Boiling Point 4265 °C7709 °F
 
Component Elements PropertiesMetricEnglishComments
Technetium, Tc 100 %100 %
 
Descriptive Properties
CAS Number7440-26-8

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ruthenium, Ru; Annealed
Silver, Ag
Strontium, Sr
Technetium, Tc; As-Rolled
Aluminum, Al

AMETc01 / 112

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.