MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LG Chemical SEETEC R3450 Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Features: Seetec R3450 is a polypropylene-ethylene random copolymer designed for the production of cast films. It has a good clarity due to the optimum content of ethylene and offers optimum balance between optical properties and physical strength. It is suitable for the skin layer of co-extruded cast film in food packaging or semi retort pouch being required high slip and medium heat seal temperature. SEETEC R3450 meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact.

Applications: CPP Film (High Slip)

CAS No. 9010-79-1

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D1505
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 82ASTM D785
Tensile Strength, Yield 260 kg(f)/cm²50mm/min; ASTM D638
Film Elongation at Break, MD >= 500 %ASTM D882
Film Elongation at Break, TD >= 500 %ASTM D882
Elongation at Break <= 500 %50mm/min; ASTM D638
Flexural Modulus 8700 kg(f)/cm²ASTM D760
Izod Impact, Notched 5.00 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
Coefficient of Friction, Static <= 0.20ASTM D1894
Film Tensile Strength at Break, MD 440 MPaASTM D882
Film Tensile Strength at Break, TD 340 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 130 - 170 °C
Crystallization Temperature 103 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °CASTM D648
Vicat Softening Point 134 °C
@Load 1.00 kg
ASTM D1525
Flash Point >= 340 °C
 
Optical PropertiesOriginal ValueComments
Haze 1.5 %ASTM D1003
Gloss 130 %45°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Heat Seal Temperature130°C>1 Kgf, LG Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical SEETEC R3400 Polypropylene Random Copolymer
LG Chemical SEETEC M1425 Polypropylene Impact Copolymer
LG Chemical SEETEC R3420 Polypropylene, Random Copolymer
LG Chemical SEETEC M1600 Polypropylene Impact Copolymer
LG Chemical SEETEC R1610 Polypropylene Random Copolymer

PLAY389 / 148399

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.