MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Braskem FLEXUS 9200 Linear low density polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: Braskem FLEXUS 9200 is a linear low density polyethylene (LLDPE) produced through metallocene catalyst which presents excellent impact and puncture strength, beyond a differential sealing performance comparing with another typical LLDPE. It processing aid and an oxidant additives.
Applications: Industrial Sacks, Blends with LDPE, Blends with HDPE, General use packing, Liners.
Processes: Blown film extrusion.

100 µm thick film, obtained from a 40 mm extruder, with blow up ratio of 2.2:1.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 960 %960 %ASTM D882
Film Elongation at Break, TD 1090 %1090 %ASTM D882
Elmendorf Tear Strength MD 780 g780 gASTM D1922
Elmendorf Tear Strength TD 1820 g1820 gASTM D1922
Dart Drop Test 1300 g2.87 lbASTM D1709
Film Tensile Strength at Break, MD 40.0 MPa5800 psiASTM D882
Film Tensile Strength at Break, TD 45.0 MPa6530 psiASTM D882
1% Secant Modulus, MD 170 MPa24700 psiASTM D882
1% Secant Modulus, TD 190 MPa27600 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 9.0 %9.0 %ASTM D1003
Gloss 100 %100 %60°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRAS610 / 314003

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.