MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SEKISUI SPI ALLEN® 3800/LXS ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Sheet

Material Notes: Co-extruded High Impact ABS Sheet (High Gloss)

ALLEN® 3800/LXS is a general purpose ABS with high impact strength.

ALLEN® 3800/LXS is Underwriters Laboratories, Inc® recognized for UL Std 94 HB (UL94) and Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302)

Suggested Applications

  • Covers and housings
  • Vehicle Interiors
  • Vehicle Exteriors with Paint or Korad
  • Marine Parts with Paint or Korad

Features:

  • Custom color matching
  • Good forming properties
  • Edge trim easily used into future orders
  • Korad can be applied for UV protection
  • High gloss finish

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 - 1.04 g/cc1.02 - 1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 34.4 MPa4990 psiASTM D638
Flexural Strength 55.8 MPa8090 psiASTM D790
Flexural Modulus 1.9994 GPa289.99 ksiASTM D790
Izod Impact, Notched  1.06 J/cm
@Temperature -17.8 °C
1.99 ft-lb/in
@Temperature 0.000 °F
ASTM D256
 3.20 J/cm
@Temperature 22.8 °C
5.99 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.5 °C195 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
Underwriters Laboratories., Inc®; Component Recognition; UL Standard 94
 
Optical PropertiesMetricEnglishComments
Gloss 85 %85 %60° Angle; ASTM D523
 
Descriptive Properties
Motor Vehicle Safety StandardPassesFMVSS 302

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Trilac® ABS-HS6500 High Impact ABS Resin
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
LG Chemical SG175G ABS, Super Surface Gloss, High Flow
LG Chemical MA201 ABS, Low Gloss
LG Chemical LG749W ABS, Low Gloss, Heat Resistance

PSEKIS011 / 185836

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.