MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Sterigenics Raprex® R-100 Branched High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Applications: Extrusion

RAPREX® R-100 is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched structure. This structure is achieved through irradiation of the polymer. It is a thermoplastic resin and is fully recyclable. Due to its broad molecular weight distribution and melt strength, RAPREX® R-100 is used for pipes, extruded profiles, sheet and large blow molded articles. Raprex® R-100 contains a robust stabilization package providing excellent melt stability as well as long-term heat aging.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.948 g/ccASTM D792
High Load Melt Index 2.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
Melt Index of Compound 0.24 g/10 min
@Load 10.0 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 34.8 MPaASTM D638
Tensile Strength, Yield 37.7 MPaASTM D638
Elongation at Break 25 %ASTM D638
Elongation at Yield 14 %ASTM D638
Flexural Modulus 1.03 GPaASTM D790
Izod Impact, Notched 160 J/mPartial Break; ASTM D256
 1.10 J/cm
@Temperature -40.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -75.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 2652 Polycarbonate
Sterigenics Raprex® R200D Branched High Density Polyethylene
Borealis FL5580 High Density Polyethylene
Asahi Kasei Leona® 1402F Nylon 66
Sterigenics Raprex® R-200 Branched High Density Polyethylene

PRAPREX6 / 65282

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.