MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nucrel® AE High Performance Adhesive and Sealant Resin
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: Nucrel® Nucrel® AE is a terpolymer of ethylene, methacrylic acid, and acrylate, available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resins. It can be used as a blend of approximately 20 to 40% Nucrel® AE with 80 to 60% LDPE for enhancement of foil adhesion properties. The level of adhesion improvement depends on processing conditions.

Characteristics:

  • Improved foil adhesion when processed under the correct conditions
  • Increased peak hot tack strength.
  • Applications:

  • Foil-containing pouches and sachets for packaging non-aggressive food and miscellaneous non-food products
  • Snack structures
  • Other foil, metallized film, or paper coatings as a heat seal or tie layer
  • Information provided by DuPont™

    This former DuPont product line is now a Dow product line.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.920 g/ccASTM D792
    Melt Flow 11 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    ASTM D1238
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 80.0 °CFreezing Point, DSC; ASTM D3418
     105 °CDSC; ASTM D3418
    Vicat Softening Point 79.0 °CASTM D1525

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
    Dow Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating
    Dow Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
    Dow Nucrel® 0908HS Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating
    Dow Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film

    PDUP961 / 33528

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.