MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin 731 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ 731 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade exhibits good surface appearance, high ductility, and good impact resistance along with low moisture absorption, creep resistance, dimensional stability, and hydrolytic stability. NORYL 731 resin is an excellent candidate for a variety of applications.

Features: Hydrolytic Stability,Low Creep Sensitivity

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Moisture Absorption 0.0600 %0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.23 %0.23 %ISO 62-1
Viscosity 8.0 cP
@Load 5.00 kg,
Temperature 280 °C
8.0 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 100 MPa14500 psiH358/30; ISO 2039-1
Tensile Strength at Break 50.0 MPa7250 psi50 mm/min; ISO 527
Tensile Strength, Yield 55.0 MPa7980 psi50 mm/min; ISO 527
Elongation at Break 30 %30 %50 mm/min; ISO 527
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527
Tensile Modulus 2.30 GPa334 ksi1 mm/min; ISO 527
Flexural Strength 75.0 MPa10900 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.20 GPa319 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 6565CS-17, 1 kg; SABIC method
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant  2.6
@Frequency 1e+6 Hz
2.6
@Frequency 1e+6 Hz
IEC 60250
 2.7
@Frequency 50.0 - 60.0 Hz
2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 19.0 kV/mm
@Thickness 3.20 mm
483 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
Dissipation Factor  0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
IEC 60250
 0.0020
@Frequency 50.0 - 60.0 Hz
0.0020
@Frequency 50.0 - 60.0 Hz
IEC 60250
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 175 V175 VIEC 60112
 250 - 400 V250 - 400 VUL 746A
Hot Wire Ignition, HWI 60 - 120 sec
@Thickness >=1.50 mm
60 - 120 sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI  15 - 30 arcs
@Thickness >=3.00 mm
15 - 30 arcs
@Thickness >=0.118 in
UL 746A
 30 - 60 arcs
@Thickness >=1.50 mm
30 - 60 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Thermal Conductivity 0.220 W/m-K1.53 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
 133 °C271 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 135 °C275 °FRate B/50; ISO 306
 140 °C284 °FRate B/120; ISO 306
 145 °C293 °FRate A/50; ISO 306
UL RTI, Electrical 105 °C221 °FUL 746B
UL RTI, Mechanical with Impact 90.0 °C194 °FUL 746B
UL RTI, Mechanical without Impact 105 °C221 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
Oxygen Index 22 %22 %ISO 4589
Glow Wire Flammability Index 750 °C
@Thickness 3.20 mm
1380 °F
@Thickness 0.126 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FCalibrator Temperature
Nozzle Temperature 260 - 280 °C500 - 536 °F
Zone 1 220 - 240 °C428 - 464 °FProfile Extrusion
Zone 2 230 - 250 °C446 - 482 °FProfile Extrusion
 260 - 280 °C500 - 536 °F
Zone 3 250 - 270 °C482 - 518 °FProfile Extrusion
 280 - 300 °C536 - 572 °F
Zone 4 250 - 270 °C482 - 518 °FProfile Extrusion
Adapter Temperature 250 - 270 °C482 - 518 °FProfile Extrusion
Die Temperature 250 - 270 °C482 - 518 °FProfile Extrusion
Melt Temperature 250 - 270 °C482 - 518 °FProfile Extrusion
 280 - 300 °C536 - 572 °FInjection Molding
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 100 - 110 °C212 - 230 °FProfile Extrusion
 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourInjection Molding
 2.00 - 3.00 hour2.00 - 3.00 hourProfile Extrusion
Precipitation Temperature 40.0 - 60.0 °C104 - 140 °FHopper Temperature
 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82243 / 290190

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.