NuSil GEL-3500 Fluorosilicone
Categories:
Polymer
;
Thermoset
;
Silicone
Material Notes:
General Purpose: Thermally Conductive
Comments: Fuel Resistant Gel, Durometer -Type '00' 50
Cure System: Platinum
Information provided by NuSil
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Viscosity
12000
cP
12000
cP
A
105000
cP
105000
cP
B
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
50
50
Hardness, Shore OO
50
50
Processing Properties
Metric
English
Comments
Cure Time
45.0
min
@Temperature 150 °C
0.750
hour
@Temperature 302 °F
Working Life
720
min
720
min
Descriptive Properties
Color
Translucent
Mix Ratio
1:1
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Rogers Arlon 31140R020 0.020" (0.508 mm) Uncured Fluorosilicone Rubber on Release Carrier
Dow Silastic® LS 4-9038 FLUOROSILICONE RUBBER
Momentive Performance Materials FQE207U Heat Cured Fluorosilicone Rubber
NuSil CF1-3510 Fluorosilicone
PNUSIL076 / 141800
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.