MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lotte Chemical Titan TITANPRO® PM655 Polypropylene homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use.

Applications: Slit tape and monofilament for rope, twine, yarn and industrial fabrics.

Advantages:

  • Outstanding process-ability.
  • Maximum bubble stability for slit tape production by the tubular process.
  • Good melt stability.
  • Superior fiber strength.
  • Low color.
  • Low taste and odor.
  • No plate out problems on die lips or chill rolls.
  • Good heat-aging stability in yarn and fabric.

Fabrication:

  • Equipment - general extrusion.
  • Techniques - standard processing for tubular and flat die tapes.

Information provided by Titan Chemicals

CAS# 9003-07-0

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Base Resin Density 0.900 g/ccASTM D1505
Water Absorption 0.020 %after 24 hrs; ASTM D570
Base Resin Melt Index 1.7 g/10 min
@Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 95ASTM D785A
Tensile Strength, Yield 35.3 MPaASTM D638
Elongation at Yield 12 %ASTM D638
Flexural Modulus 1.72 GPaASTM D790B
Izod Impact, Notched 53.9 J/mASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lotte Chemical Titan TITANPRO® PD855 Polypropylene homopolymer
Lotte Chemical Titan TITANPRO® PM803 Polypropylene homopolymer
Lotte Chemical Titan TITANPRO® PX617 Polypropylene homopolymer
Lotte Chemical Titan TITANPRO® PD701 Polypropylene homopolymer
Lotte Chemical Titan TITANPRO® PM383 Polypropylene homopolymer

PTITAN02 / 70368

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.